Silicon carbon alloy, also known as high carbon silicon alloy, is an alloy composed of silicon and carbon, with a higher carbon content compared to ferrosilicon. It is a new type of alloy used in converter steelmaking, which can completely replace carbon enhancers and deoxidizers. Due to its high density, high carbon silicon alloy can be added to molten steel in block form, effectively acting as a deoxidizer and significantly improving the carbon recovery rate (which can exceed 98%).
High carbon silicon alloy can improve the quality of molten steel, enhance product quality and new functionalities, reduce the number of alloy additions, lower steelmaking costs, increase economic benefits, greatly improve environmental conditions, and reduce worker labor intensity.


High Carbon Silicon Alloy Deoxidation Mechanism
Oxygen exists in molten steel in the form of ferrous oxide (FeO). If the molten steel contains a large amount of FeO, gas pores can form during the solidification process, reducing the strength and plasticity of the steel and severely affecting its mechanical properties. Therefore, effective deoxidation is necessary during steelmaking. Traditionally, pure aluminum is used as a deoxidizer, but due to its low density and tendency to float, its utilization rate is low, which increases consumption and production costs. Additionally, aluminum has a low melting point and high specific heat capacity, further complicating its use.
Composition of High Carbon Silicon Alloy
High carbon silicon alloy consists of the following components by weight percentage: silicon 50-68%, carbon 15-20%, phosphorus ≤0.05%, sulfur ≤0.05%.
Preparation Method of High Carbon Silicon Alloy
- Basic Process: Steel preparation—smelting—slag removal—ingot casting—testing—ingredient adjustment—remelting—adding aluminum ingots—stirring—slag removal—heat preservation—casting into blocks.
- Simplified Process: When the steel composition is relatively certain, the remelting step can be omitted: steel preparation—smelting—adding aluminum ingots—stirring—slag removal—heat preservation—casting into blocks.
High Carbon Silicon Alloy Preparation Process Description
- Steel Material: Scrap steel can be used with an appropriate amount of ferrosilicon. The scrap steel needs to be shot-blasted to remove rust before smelting.
- Smelting: Scrap steel is melted at temperatures above 1570°C before adding ferrosilicon.
- Casting: The molten steel is heated to above 1600°C, and then carbon is added, stirred, degassed, deoxidized, and heat-preserved before quickly casting at temperatures of 1250-1280°C.
Advantages of High Carbon Silicon Alloy
- Strong Deoxidation: With silicon content above 50%, it has a strong deoxidation effect and does not contain manganese, making it widely applicable.
- High Utilization Rate: Its high density allows it to penetrate the molten steel and fully deoxidize.
- Cost-Effective: Compared to pure aluminum, production costs are significantly lower, and using scrap steel can further reduce costs.
- Stable Composition: The remelting process allows for precise adjustment of the alloy composition, ensuring reliable chemical properties and preventing the inclusion of harmful elements and impurities.
- Good Casting Properties: High carbon content ensures strong fluidity and good mold filling during casting.
- Multi-Functional Applications: Besides deoxidation, it can also be used with inoculants to enhance steel quality.
High Carbon Silicon Example Implementation
Equipment: 160KW thyristor intermediate frequency induction furnace with a melting capacity of 150kg.
High Carbon Silicon Preparation Process
- Prepare 88kg of scrap steel and 1kg of 75FeSi: The scrap steel is shot-blasted to remove rust.
- Melt Scrap Steel: When the temperature exceeds 1570°C, add ferrosilicon.
- Molten Steel Treatment: After slag removal, pour the molten steel into ingots, test the composition (C 0.40%, Si 1.20%, P 0.05%, S 0.04%, Fe balance), and adjust before remelting.
- Add Carbon 71kg: Heat the molten steel to above 1600°C, add carbon, stir, degas, deoxidize, heat-preserve, and quickly cast at temperatures of 1250-1280°C.
Through trials, a high carbon silicon alloy deoxidizer was obtained.
High carbon silicon alloy, as an efficient and cost-effective intermediate alloy deoxidizer for steelmaking, offers new solutions for the steel industry, with broad application prospects and economic benefits.