A Leading Ferro Alloy Manufacturer

What is the production method of low carbon ferrochrome?

Home » News » What is the production method of low carbon ferrochrome?
Medium, low, and micro-carbon ferrochrome

Share

Low carbon ferrochrome is produced by mixing chromite and iron in an electric arc furnace. It is widely used in the casting and steel industries, particularly in the production of low carbon structural steel, chromium steel, and alloy structural steel. Based on carbon content, ferrochrome alloys can be classified into high carbon ferrochrome, medium carbon ferrochrome, low carbon ferrochrome, and micro carbon ferrochrome.

What is Low Carbon Ferrochrome?

Low carbon ferrochrome is a type of ferrochrome with a carbon content below 0.50%. The raw materials for producing low carbon ferrochrome include silicon chromium alloy, chromite, limestone, and other metallurgical materials. It is used in various industries and is a necessary additive in the production of stainless steel and special steel, improving the oxidation and corrosion resistance of steel.

BrandCrC maxSi maxP maxS max
FeCr65C0.2560-700.251.50.030.025
FeCr55C0.2560-700.252.00.040.03
FeCr65C0.5060-700.501.50.030.025
FeCr55C0.5060-700.502.00.040.03
Low Carbon Ferrochrome Brand
Low carbon ferrochrome
Ferrochrome alloy

Smelting Methods for Low Carbon Ferrochrome

There are currently two main smelting methods for low carbon ferrochrome: the high carbon ferrochrome refining method and the electro-silicon thermal method.

High Carbon Ferrochrome Refining Method

The high carbon ferrochrome refining method is divided into chromite refining high carbon ferrochrome and oxygen refining high carbon ferrochrome.

Chromite Refining High Carbon Ferrochrome

When using chromite to refine high carbon ferrochrome, the slag in the refining furnace has high viscosity and a high melting point, requiring very high temperatures. This results in high power consumption, short lining life, and difficulty in reducing carbon content. In contrast, oxygen refining high carbon ferrochrome offers significant advantages, including high productivity, low production costs, and a high recovery rate.

Oxygen Blowing Low Carbon Ferrochrome

The raw materials for oxygen top-blown refining of low carbon ferrochrome include high carbon ferrochrome, chromite, lime, and silicon chromium alloy. The liquid high carbon ferrochrome in the converter usually requires a temperature between 1723 and 1873K. The molten iron contains over 60% chromium, less than 1.5% silicon, and less than 0.036% sulfur. Chromite is used as a slagging material, with a low SiO3 content and higher MgO and Al2O3 content to avoid high viscosity. Lime, with similar requirements to those in the electrosilicon thermal process, is also used as a slagging material. Si-Cr alloy is used to reduce high chromium slag in the later stages of blowing, typically in powder form after crushing.

The equipment for producing low carbon ferrochrome by oxygen blowing is a converter, so this method is called the converter method. Oxygen supply methods can vary, including side blowing, top blowing, bottom blowing, and top-bottom blowing. In China, the top-blown converter method is used. Oxygen is directly blown into the high carbon ferrochrome liquid to decarburize and produce low carbon ferrochrome. The main elements in high carbon ferrochrome are chromium, iron, silicon, and carbon, which are all oxidizable. During oxidation and smelting, the primary task is to decarburize while preserving chromium. As chromium and iron make up over 90% of the alloy, they are oxidized first, followed by silicon oxidation. The oxidation of these elements increases the molten pool temperature rapidly, accelerating the decarburization reaction. Higher temperatures favor the decarburization reaction and inhibit chromium oxidation, reducing the carbon content in the alloy.

Electrosilicon Thermal Method for Smelting Low Carbon Ferrochrome

The electro-silicon thermal method involves reducing chromium and iron oxides in chromite using silicon from silicon chromium alloy under basic slag conditions in an electric furnace.

Smelting Equipment and Raw Materials

Smelting low carbon ferrochrome using the silicon thermal method is done in a fixed three-phase electric arc furnace, which can use self-baking electrodes. The furnace lining is made with magnesium brick (dry lining). A significant issue in low carbon ferrochrome production is the short lining life due to high smelting temperatures (up to 1650 degrees Celsius). The raw materials for smelting low carbon ferrochrome include chromite, silicon-chromium alloy, and lime. Chromite should be a dry, pure block ore or refined powder with a high Cr2O3 content and low impurities (Al2O3, MgO, SiO2). Phosphorus content should be no more than 0.03%, and the particle size should be less than 60mm. The Si-Cr alloy should be crushed to a particle size of less than 30mm, with no residue. Lime should be freshly burned with more than 85% CaO content.

Low carbon ferrochrome is not only widely used but also involves a sophisticated production process, showcasing the intricacies and advancements in metallurgical techniques.